PREPARATION AND PROPERTIES OF COMPOSITETiO2MACROPOROUS COPOLYMER AND ITS APPLICATION FOR EXPANDED BED ADSORPTION (Ⅱ) EXPANSION CHARACTERISTICS,LIQUID MIXING ANDADSORPTION PERFORMANCE
QIAN Jianhua, LEI Yinlin, LIU Zuozhen, et al. PREPARATION AND PROPERTIES OF COMPOSITETiO2MACROPOROUS COPOLYMER AND ITS APPLICATION FOR EXPANDED BED ADSORPTION (Ⅱ) EXPANSION CHARACTERISTICS,LIQUID MIXING ANDADSORPTION PERFORMANCE[J]. CIESC Journal, 2004, (1): 9-14.
QIAN Jianhua, LEI Yinlin, LIU Zuozhen, et al. PREPARATION AND PROPERTIES OF COMPOSITETiO2MACROPOROUS COPOLYMER AND ITS APPLICATION FOR EXPANDED BED ADSORPTION (Ⅱ) EXPANSION CHARACTERISTICS,LIQUID MIXING ANDADSORPTION PERFORMANCE[J]. CIESC Journal, 2004, (1): 9-14.DOI:
the GET composite copolymer with pendant epoxy groups were prepared. It was reacted with diethylamine
forming an anion-exchange chromatographic medium DEAE-GET. The effects of liquid viscosity
flow velocity on expansion characteristics and liquid mixing performance of DEAE-GET in expanded bed were studied. Its expansion characteristics in STREAMLINE 25 column were found to obey the Richardson-Zaki equation. The increase of liquid viscosity
flow velocity resulted in the increase of axial mixing coefficient. In the range of flow velocity 100—500 cm8226;h-1
the low value of axial mixing coefficient in expanded bed (10-6—10-5m28226;s-1) indicated that the liquid flow through the expanded bed was close to a plug flow profile. The maximum static adsorption capacity for BSA was found to be 43.0 mg8226;ml-1.The breakthrough curves for BSA adsorption on DEAE-GET and STREAMLINE DEAE in packed bed and expanded bed were compared
showing for each adsorbent they were close to each other.The maximum adsorption capacities on DEAE-GET in packed bed and expanded bed were 28.0 mg8226;ml-1 and 26.2 mg8226;ml-1 respectively.