The porous electrodes were made by admixing PTFE emulsion with carbon black. In the electrolytic cell the cathode and the anode were separated by a ration exchange membrane. The current efficiency of HO2- exceeded 90% at the temperature of 20℃
when the concentration of KOH was greater than 0.3mol/l
the power consumption was 2.2kW·h per kg of H2O2. The steadystate polarization curve was measured.