FLUORIDE EMISSION CONTROL BY BLENDING AND INJECTING CaO AND CALCIUM-BASED SORBENTS DURING COAL COMBUSTION
|更新时间:2025-12-10
|
FLUORIDE EMISSION CONTROL BY BLENDING AND INJECTING CaO AND CALCIUM-BASED SORBENTS DURING COAL COMBUSTION
CIESC JournalIssue 2, Pages: 226-231(2003)
作者机构:
浙江大学热能工程研究所能源洁净利用与环境工程教育部重点实验室
作者简介:
基金信息:
DOI:
CLC:
Online First:25 February 2003,
Published:25 February 2003
稿件说明:
移动端阅览
QI Qingjie, LIU Jianzhong, ZHOU Junhu, et al. FLUORIDE EMISSION CONTROL BY BLENDING AND INJECTING CaO AND CALCIUM-BASED SORBENTS DURING COAL COMBUSTION[J]. CIESC Journal, 2003, (2): 226-231.
DOI:
QI Qingjie, LIU Jianzhong, ZHOU Junhu, et al. FLUORIDE EMISSION CONTROL BY BLENDING AND INJECTING CaO AND CALCIUM-BASED SORBENTS DURING COAL COMBUSTION[J]. CIESC Journal, 2003, (2): 226-231.DOI:
FLUORIDE EMISSION CONTROL BY BLENDING AND INJECTING CaO AND CALCIUM-BASED SORBENTS DURING COAL COMBUSTION
The experimental and theoretical analysis about toxic fluoride removal during coal combustion are reported in this paper.It has been identified that CaO can restrain the emission of fluoride and fluoride retention ratios are between 12.2% and 61.0%
with mean value 39.5% by blending CaO with coal during coal combustion in tubular furnace at 900 ℃. Influence factors on fluoride retention by blending CaO with coal are studied such as type of coals
combustion temperature
retention time and Ca/S molar ratio.The optimum conditions for fluoride retention by blending CaO with coal are that combustion temperature in the range 800 to 1000 ℃
retention time between 5—10 min and Ca/S ratio in the range 2.5 to 3.0. In chain-grate furnace combustion of coal
fluoride retention ratios are about 54.0%—64.8% with mean value 59.3% by blending calcium-based sorbents with coal and are about 72.5%—80.5% with mean value 75.5% by blending calcium-based sorbents with coal accompanied by injection of calcium-based sorbents.